Structure 9010149

9010148 << 9010149 >> 9010150
Original COD entry Download CIF Download DOT

Citation: Post, J. E.; Bish, D. L.; Heaney, P. J. (2007). Synchrotron powder X-ray diffraction study of the structure and dehydration behavior of sepiolite Sample: T = 742 K. American Mineralogist, 92, pp. 91-97.

Formula: H2 Mg2 O9 Si3

Cell parameters:

  • a = 23.446 Å
  • b = 11.352 Å
  • c = 5.2782 Å
  • α = 90°
  • β = 89.06°
  • γ = 90°

List type: noninterleaving

List: 3D

Combined 3D structure and graph

span 1 {1 1 1}
Ctrl-click to select multiple nodes

JSmol combined CIF view

Linear Graph Knot

Molecules